bloating

Firing defect where blisters form within claybody, raising large lumps on the surface. Caused by expansion of gases within clay, as a result of excessive early reduction (trapped carbon—carbon coring), excessively fast bisque-firing (trapped carbon and sulfur), or overfiring (volatization of fluxes).